B.  Method No. 405B: Heavy Corrosion, Hard Carbon, Paint, and Scale Removal..................426

C.  Method No. 405C: Seal Diameter (Lip Seal Surface) Repair Using Glass Bead Peening .. 426
6. Repairing Magnesium Parts......................................................................................................... 427

A.  Method No. 406A: Minor Damage Repair ............................................................................ 427

B.  Method No. 406B: Heavy Damage Repair...........................................................................428

C.  Method No. 406C: Gouge and Scoring Repair .................................................................... 429

7. Replacing Inserts, Studs, Bushings, and Pins.............................................................................430

A.  Method No. 407A: Loose or Damaged Thread Inserts Replacement..................................430

B.  Method No. 407B: Loose or Damaged Thread Inserts (Aluminum or Magnesium Parts) Replacement ......................................................................................................................... 436
C.  Method No. 407C: Loose or Damaged Keensert Stud Repair.............................................436

D.  Method No. 407D: Loose, Worn, or Damaged Bushings (Steel Parts) Replacement ......... 438

E.  Method No. 407E: Loose, Worn, or Damaged Bushings (Aluminum or Magnesium Parts) Replacement...............................................................................................................438
F.  Method No. 407F: Loose, Worn, or Damaged Pins (Steel Parts) Replacement.................. 439

G.  Method No. 407G: Loose, Worn, or Damaged Pins (Aluminum or Magnesium Parts) Replacement ......................................................................................................................... 440
H.  Method No. 407H: Loose, Worn, or Damaged Rosan Stud and Insert Replacement ......... 440

8. Repairing Gear Teeth .................................................................................................................. 443

A.  Method No. 408A: Minor Gear Teeth Involute Surface Damage Repair ............................. 443

Page TC-3
Apr 1/05
20-00-02/70-00-01
Copying, use or disclosure of information on this page is subject to proprietary restrictions.

SECTION  PAGE
9. Repainting Parts........................................................................................................................... 443

A.  Method No. 409A: Alloy Part Painted Surface (Enamel) Repair..........................................443

B.  Method No. 409B: Alloy Part Painted Surface (Color-coat) Repair ..................................... 444

10. Repairing Riveted Parts ............................................................................................................... 444

A.  Method No. 410A: Damaged Rivet Replacement General Guidelines ................................ 444

B.  Method No. 410B: Damaged Rivet Replacement ................................................................ 445

11. Repairing Welded Parts ............................................................................................................... 446

A.  Method No. 411A: Fusion Weld Repair of Aluminum Alloy Parts ........................................ 446

B.  Method No. 411B: Fusion Weld Repair of Magnesium Alloy Parts...................................... 446

C.  Method No. 411C: Fusion Weld Repair of Corrosion-Resistant Steels Cobalt- And Nickel-Base Alloy Parts ......................................................................................................... 447
12. Balancing Procedures and Guidelines......................................................................................... 448
 